| 断裂伸长率 | 650% | 拉伸强度 | 27MPa | 密度 | 0.929g/cm3 |
| 熔体流动速率 | 0.3g/10min | 维卡软化点 | 73℃ | 用途级别 | 薄膜级 |
| 规格级别 | 薄膜 |
|
|
产品简述
| 断裂伸长率 | 650% | 拉伸强度 | 27MPa | 密度 | 0.929g/cm3 |
| 熔体流动速率 | 0.3g/10min | 维卡软化点 | 73℃ | 用途级别 | 薄膜级 |
| 规格级别 | 薄膜 |
详细数据
订购指南
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||||
| 基本性能 | 比重 | ASTM D-1505 | 0.929 | g/cm3 | ||||
| 熔体质量流动速率 | 190℃/2.16kg | ASTM D-1238 | 0.30 | g/10min | ||||
| VA含量 | 12 | wt% | ||||||
| 机械性能 | 耐环境应力开裂性 | 100% lgepal F50 | ASTM D-1693 | >300 | Hr | |||
| 拉伸屈服强度 | ASTM D-638 | 6 | MPa | |||||
| 拉伸断裂强度 | ASTM D-638 | 27 | MPa | |||||
| 断裂伸长率 | ASTM D-638 | 650 | % | |||||
| 摩擦系数 | ASTM D-1894 | >1.0 | ||||||
| 拉伸屈服强度 | 30.0µm | ASTM D-882 |
|
MPa | ||||
| 拉伸断裂强度 | 30.0µm | ASTM D-882 |
|
MPa | ||||
| 断裂伸长率 | 30.0µm | ASTM D-882 |
|
% | ||||
| 埃尔曼多夫撕裂强度 | 0.0300mm | ASTM D-1922 |
|
kN/m | ||||
| 热性能 | 脆化温度 | ASTM D-746 | <-50 | ℃ | ||||
| 维卡软化温度 | ASTM D-1525 | 73 | ℃ | |||||
| 熔化温度 | ASTM D-3418 | 95 | ℃ | |||||
| 光学性能 | 光泽度 | 60° | ASTM D-2457 | 53 | ||||
| 雾度 | 30.0µm | ASTM D-1003 | 10 | % | ||||