| 断裂伸长率 | 900% | 拉伸强度 | 30MPa | 密度 | 0.963g/cm3 |
| 熔体流动速率 | 0.73g/10min | 加工级别 | 注塑级 | 特性级别 | 耐高温 |
|
|
产品简述
| 断裂伸长率 | 900% | 拉伸强度 | 30MPa | 密度 | 0.963g/cm3 |
| 熔体流动速率 | 0.73g/10min | 加工级别 | 注塑级 | 特性级别 | 耐高温 |
详细数据
订购指南
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
| 基本性能 | 熔体流动速率 | ASTM D-1238 | 0.73 | g/10min | ||
| 密度 | ASTM D-4883 | 0.963 | g/cm3 | |||
| 屈服拉伸强度 | MD | ASTM D-882 | 39 | MPa | ||
| TD | ASTM D-882 | 35 | MPa | |||
| 机械性能 | 断裂拉伸强度 | MD | ASTM D-882 | 37 | MPa | |
| TD | ASTM D-882 | 30 | MPa | |||
| 屈服伸长率 | MD | ASTM D-882 | 9 | % | ||
| TD | ASTM D-882 | 9 | % | |||
| 断裂伸长率 | MD | ASTM D-882 | 900 | % | ||
| TD | ASTM D-882 | 900 | % | |||
| 1%正割模量 | MD | ASTM D-882 | 1030 | MPa | ||
| TD | ASTM D-882 | 1100 | MPa | |||
| 埃尔曼多夫撕裂强度 | MD | ASTM D-1922 | 5 | N/mm2 | ||
| TD | ASTM D-1922 | 96 | N/mm2 | |||
| 冲击强度 | 35 | g | ||||