| 断裂伸长率 | 500% | 拉伸强度 | 56MPa | 密度 | 0.952g/cm3 | 
| 熔体流动速率 | 0.05g/10min | 维卡软化点 | 125℃ | 用途级别 | 薄膜级 | 
| 规格级别 | 薄膜 | 加工级别 | 挤出级 | 特性级别 | 高强度 | 
				
					
		| 
				
				
				
				 | 
			
			
产品简述
| 断裂伸长率 | 500% | 拉伸强度 | 56MPa | 密度 | 0.952g/cm3 | 
| 熔体流动速率 | 0.05g/10min | 维卡软化点 | 125℃ | 用途级别 | 薄膜级 | 
| 规格级别 | 薄膜 | 加工级别 | 挤出级 | 特性级别 | 高强度 | 
详细数据
订购指南
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
| 基本性能 | HLMI | ASTM D-1238 | 9 | g/10min | ||
| 密度 | ASTM D-1505 | 0.952 | g/cm3 | |||
| 熔体流动速率 | 0.05 | g/10min | ||||
| 机械性能 | 拉伸断裂伸长率 | MD | ASTM D-882 | 400 | % | |
| TD | ASTM D-882 | 500 | % | |||
| 门氏撕裂强度 | MD | 12 | g | |||
| TD | 60 | g | ||||
| 1%割线模量 | MD | ASTM D-882 | 1250 | MPa | ||
| TD | ASTM D-882 | 1500 | MPa | |||
| 拉伸断裂强度 | MD | ASTM D-882 | 60 | MPa | ||
| TD | ASTM D-882 | 56 | MPa | |||
| 拉伸屈服强度 | MD | ASTM D-1505 | 33 | MPa | ||
| TD | ASTM D-1505 | 31 | MPa | |||
| Dart冲击强度 | F50 | ASTM D-1709 | 180 | g | ||
| 热性能 | 维卡软化点 | ASTM D-1525 | 125 | ℃ | ||