| 断裂伸长率 | 650% | 拉伸强度 | 11MPa | 密度 | 0.923g/cm3 |
| 熔体流动速率 | 4g/10min | 用途级别 | 薄膜级,纤维 | 规格级别 | 薄膜 |
| 缺口冲击强度 | 60 | 加工级别 | 注塑级 | 特性级别 | 增强级 |
|
|
产品简述
| 断裂伸长率 | 650% | 拉伸强度 | 11MPa | 密度 | 0.923g/cm3 |
| 熔体流动速率 | 4g/10min | 用途级别 | 薄膜级,纤维 | 规格级别 | 薄膜 |
| 缺口冲击强度 | 60 | 加工级别 | 注塑级 | 特性级别 | 增强级 |
详细数据
订购指南
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
| 基本性能 | 熔体流动速率 | ASTM D-1238 | 4.0 | g/10min | ||
| 密度 | ASTM D-1505 | 0.923 | g/cc | |||
| 机械性能 | 延伸率(破断点) | ASTM D-638 | 650 | % | ||
| 拉伸抗热强度 | MD | ASTM D-1004 | 90 | kg/cm | ||
| TD | ASTM D-1004 | 85 | kg/cm | |||
| 抗张强度(破断点) | ASTM D-638 | 115 | kg/cm2 | |||
| 下降冲击强度 | ASTM D1709 | 60 | g | |||
| 断裂伸长率 | MD | ASTM D-882 | 350 | % | ||
| TD | ASTM D-882 | 550 | % | |||
| 断裂拉伸强度 | MD | ASTM D-882 | 210 | kg/cm2 | ||
| TD | ASTM D-882 | 180 | kg/cm2 | |||
| 热性能 | 熔点 | ASTM D-2117 | 111 | ℃ | ||
| 维卡软化点 | ASTM D-1525 | 87 | ℃ | |||
| 其它性能 | 厚度 | HCC | 0.03 | ㎜ | ||
| 光泽度 | 45℃ | ASTM D-2457 | 80 | % | ||
| 混浊度 | ASTM D-1009 | 4.0 | % | |||