| 断裂伸长率 | 200% | 拉伸强度 | 10.9MPa | 密度 | 0.924g/cm3 |
| 熔体流动速率 | 3g/10min | 规格级别 | 吹塑 | 加工级别 | 吹塑级 |
| 特性级别 | 透明级,抗化学性 |
|
|
产品简述
| 断裂伸长率 | 200% | 拉伸强度 | 10.9MPa | 密度 | 0.924g/cm3 |
| 熔体流动速率 | 3g/10min | 规格级别 | 吹塑 | 加工级别 | 吹塑级 |
| 特性级别 | 透明级,抗化学性 |
详细数据
订购指南
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||||
| 基本性能 | 密度 | ASTM D-1505 | 0.924 | g/cm3 | ||||
| 熔体流动速率 | 190℃/2.16kg | ASTM D-1238 | 3 | g/10min | ||||
| 机械性能 | 薄膜厚度-Tested | 31.8 | um | |||||
| 割线模量-1% Secant | 31.8um,Blown Film | ASTM D-882 |
|
MPa | ||||
| 割线模量-1% Secant | 31.8um,Cast Film | ASTM D-882 |
|
MPa | ||||
| 拉抻屈服强度 | 31.8um,Blown Film | ASTM D-882 |
|
MPa | ||||
| 拉抻屈服强度 | 31.8um,Cast Film | ASTM D-882 |
|
MPa | ||||
| 拉抻断裂强度 | 31.8um,Blown Film | ASTM D-882 |
|
MPa | ||||
| 拉抻断裂强度 | 31.8um,Cast Film | ASTM D-882 |
|
MPa | ||||
| 拉伸断裂伸长率 | 31.8um,Blown Film | ASTM D-882 |
|
% | ||||
| 拉伸断裂伸长率 | 31.8um,Cast Film | ASTM D-882 |
|
% | ||||
| 落锤冲击 | 31.8um,Blown Film | ASTM D-1709 | 65 | g | ||||
| 落锤冲击 | 31.8um,Cast Film | ASTM D-1709 | 110 | g | ||||
| 埃尔曼多夫撕裂强度 | 31.8um,Blown Film | ASTM D-1922 |
|
g | ||||
| 埃尔曼多夫撕裂强度 | 31.8um,Cast Film | ASTM D-1922 |
|
% | ||||
| 光学性能 | 光泽度 | 45°,38.1um,Blown Film | ASTM D-2457 | 70 | ||||
| 光泽度 | 45°,31.8um,Cast Film | ASTM D-2457 | 77 | |||||
| 雾度 | 31.7um,Blown Film | ASTM D-1003 | 5.4 | % | ||||
| 雾度 | 31.7um,Cast Film | ASTM D-1003 | 3.4 | % | ||||