| 断裂伸长率 | 760% | 拉伸强度 | 33MPa | 密度 | 0.92g/cm3 | 
| 熔体流动速率 | 1g/10min | 维卡软化点 | 93℃ | 用途级别 | 薄膜级,食品级 | 
| 规格级别 | 薄膜 | 
				
					
		| 
				
				
				
				 | 
			
			
产品简述
| 断裂伸长率 | 760% | 拉伸强度 | 33MPa | 密度 | 0.92g/cm3 | 
| 熔体流动速率 | 1g/10min | 维卡软化点 | 93℃ | 用途级别 | 薄膜级,食品级 | 
| 规格级别 | 薄膜 | 
详细数据
订购指南
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
| 基本性能 | 熔体流动速率 | ASTM D-1238 | 1.0 | g/10min | ||
| 密度 | ASTM D-1505 | 0.920 | g/cm3 | |||
| 机械性能 | 1%伸长弹性系数 | MD | ASTM D-882B | 1900 | kg/cm2 | |
| TD | ASTM D-882B | 2400 | kg/cm2 | |||
| 拉力断裂强度 | MD | ASTM D-882B | 420 | kg/cm2 | ||
| TD | ASTM D-882B | 340 | kg/cm2 | |||
| 拉力断裂伸长率 | MD | ASTM D-882B | 580 | % | ||
| TD | ASTM D-882B | 760 | % | |||
| 落球冲击强度 | ASTM D-1709 | 260 | g | |||
| 抗撕裂性 | MD | ASTM D-1922 | 240 | g/25µm | ||
| TD | ASTM D-1922 | 540 | g/25µm | |||
| 拉力降伏强度 | MD | ASTM D-882B | 105 | kg/cm2 | ||
| TD | ASTM D-882B | 110 | kg/cm2 | |||
| 热性能 | 熔点 | DSC | 122 | ℃ | ||
| 软化点 | ASTM D-1525 | 93 | ℃ | |||
| 脆化温度 | ASTM D-746 | <-70 | ℃ | |||
| 其它性能 | 透明度 | 60 | % | |||
| 抗粘剂 | 高 | |||||
| 光泽度 | 45℃ | ASTM D-2457 | 51 | % | ||
| 浊度 | ASTM D-1003 | 15 | % | |||
| 滑剂 | 高 | |||||