| 断裂伸长率 | 800% | 拉伸强度 | 34MPa | 密度 | 0.919g/cm3 |
| 熔体流动速率 | 1g/10min | 维卡软化点 | 102℃ | 用途级别 | 薄膜级,纤维 |
| 规格级别 | 薄膜 | 加工级别 | 注塑级 | 特性级别 | 增强级 |
|
|
产品简述
| 断裂伸长率 | 800% | 拉伸强度 | 34MPa | 密度 | 0.919g/cm3 |
| 熔体流动速率 | 1g/10min | 维卡软化点 | 102℃ | 用途级别 | 薄膜级,纤维 |
| 规格级别 | 薄膜 | 加工级别 | 注塑级 | 特性级别 | 增强级 |
详细数据
订购指南
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
| 基本性能 | 密度 | ASTM D-1505 | 0.919 | g/cm3 | ||
| 熔体流动速率 | ASTM D-1238 | 1.0 | g/10min | |||
| 物理性能 | 薄膜厚度 | 25 | μm | |||
| 机械性能 | 尖头冲击强度 | ASTM D-1709 | 3.7 | g/μm | ||
| 断裂伸长率 | MD | ASTM D-882 | 650 | % | ||
| TD | ASTM D-882 | 800 | % | |||
| 屈服拉伸强度 | MD | ASTM D-882 | 120 | Kg/cm2 | ||
| TD | ASTM D-882 | 110 | Kg/cm2 | |||
| 抗张模数 | MD | ASTM D-882 | 2000 | Kg/cm2 | ||
| TD | ASTM D-882 | 2500 | Kg/cm2 | |||
| 断裂拉伸强度 | MD | ASTM D-882 | 400 | Kg/cm2 | ||
| TD | ASTM D-882 | 350 | Kg/cm2 | |||
| 撕裂强度 | MD | ASTM D-1004 | 125 | kg/cm | ||
| TD | ASTM D-1004 | 105 | kg/cm | |||
| 热性能 | 软化点 | ASTM D-1525 | 102 | ℃ | ||
| 低温脆化温度 | ASTM D-746 | <-70 | ℃ | |||