| 断裂伸长率 | 830% | 拉伸强度 | 33MPa | 密度 | 0.92g/cm3 |
| 熔体流动速率 | 2g/10min |
|
|
产品简述
| 断裂伸长率 | 830% | 拉伸强度 | 33MPa | 密度 | 0.92g/cm3 |
| 熔体流动速率 | 2g/10min |
详细数据
订购指南
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
| 基本性能 | 密度 | ASTM D-1505 | 0.920 | g/cm3 | ||
| 熔体流动速率 | ASTM D-1238 | 2.0 | g/10min | |||
| 物理性能 | 薄膜厚度 | ASTM D-374 | 30 | μm | ||
| 机械性能 | 断裂伸长率 | MD | ASTM D-882 | 800 | % | |
| TD | ASTM D-882 | 830 | % | |||
| 拉伸模量 | MD | ASTM D-882 | 2200 | kg/cm2 | ||
| TD | ASTM D-882 | 2700 | kg/cm2 | |||
| 冲击强度 | ASTM D-1709 | 115 | g | |||
| 断裂拉伸强度 | MD | ASTM D-882 | 370 | kg/cm2 | ||
| TD | ASTM D-882 | 340 | kg/cm2 | |||
| 埃门多夫撕裂强度 | MD | ASTM D-1922 | 4 | g/μm | ||
| TD | ASTM D-1922 | 7 | g/μm | |||
| 拉伸屈服强度 | MD | ASTM D-882 | 112 | kg/cm2 | ||
| TD | ASTM D-882 | 112 | kg/cm2 | |||
| 其它性能 | 雾度 | ASTM D-1003 | 2 | % | ||