| 断裂伸长率 | 800% | 拉伸强度 | 33MPa | 密度 | 0.919g/cm3 | 
| 熔体流动速率 | 2g/10min | 维卡软化点 | 102℃ | 用途级别 | 薄膜级,电线电缆级 | 
| 规格级别 | 高光泽薄膜吹塑 | 加工级别 | 吹塑级 | 特性级别 | 高光泽 | 
				
					
		| 
				
				
				
				 | 
			
			
产品简述
| 断裂伸长率 | 800% | 拉伸强度 | 33MPa | 密度 | 0.919g/cm3 | 
| 熔体流动速率 | 2g/10min | 维卡软化点 | 102℃ | 用途级别 | 薄膜级,电线电缆级 | 
| 规格级别 | 高光泽薄膜吹塑 | 加工级别 | 吹塑级 | 特性级别 | 高光泽 | 
详细数据
订购指南
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
| 基本性能 | 密度 | ASTM D-1505 | 0.919 | g/cm3 | ||
| 物理性能 | 熔体流动速率 | ASTM D-1238 | 2.0 | g/10min | ||
| 薄膜厚度 | 25 | μm | ||||
| 机械性能 | 抗张强度(屈服点) | MD | ASTM D-882 | 120 | Kg/cm2 | |
| TD | ASTM D-882 | 110 | Kg/cm2 | |||
| 断裂伸长率 | MD | ASTM D-882 | 650 | % | ||
| TD | ASTM D-882 | 800 | % | |||
| 抗张强度(断裂点) | MD | ASTM D-882 | 380 | Kg/cm2 | ||
| TM | ASTM D-882 | 340 | Kg/cm2 | |||
| 抗张模数 | MD | ASTM D-882 | 2000 | Kg/cm2 | ||
| TD | ASTM D-882 | 2500 | Kg/cm2 | |||
| 撕裂强度 | MD | ASTM D-1004 | 125 | Kg/cm | ||
| TD | ASTM D-1004 | 105 | Kg/cm | |||
| 尖头冲击强度 | ASTM D-1709 | 3.7 | g/μm | |||
| 热性能 | 低温脆化温度 | ASTM D-746 | <-70 | ℃ | ||
| 软化点 | ASTM D-1525 | 102 | ℃ | |||