| 断裂伸长率 | 800% | 拉伸强度 | 39MPa | 密度 | 0.92g/cm3 |
| 熔体流动速率 | 2g/10min | 用途级别 | 薄膜级,食品级 | 规格级别 | 薄膜 |
| 脆化温度 | -70℃ | 特性级别 | 透明级 |
|
|
产品简述
| 断裂伸长率 | 800% | 拉伸强度 | 39MPa | 密度 | 0.92g/cm3 |
| 熔体流动速率 | 2g/10min | 用途级别 | 薄膜级,食品级 | 规格级别 | 薄膜 |
| 脆化温度 | -70℃ | 特性级别 | 透明级 |
详细数据
订购指南
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
| 基本性能 | 密度 | ASTM D-1505 | 0.920 | g/cm3 | ||
| 熔体流动速率 | ASTM D-1238 | 2.00 | g/10min | |||
| 物理性能 | 光泽度 | 45℃ | ASTM D-2457 | 92 | ||
| 雾度 | ASTM D-1003 | 1.0 | % | |||
| 薄膜厚度 | HYUNDAI | 25 | um | |||
| 机械性能 | 撕裂伸长率 | MD | ASTM D-882 | 700 | % | |
| TD | ASTM D-882 | 800 | % | |||
| 撕裂强度 | MD | TEAR LENGTH 21.5mm | ASTM D-1992 | 70 | % | |
| TD | TEAR LENGTH 21.5mm | ASTM D-1992 | 210 | % | ||
| 撕裂拉伸强度 | MD | ASTM D-882 | 450 | kg/cm2 | ||
| TD | ASTM D-882 | 400 | kg/cm2 | |||
| 落球冲击强度 | ASTM D-1709 | 130 | g | |||
| 热性能 | 低温脆点 | ASTM D-746 | <-70 | ℃ | ||