| 加工级别 | 注塑级 | 特性级别 | 阻燃级,增强级 | 用途级别 | 汽车部件,电子电器部件,家电部件 |
|
|
产品简述
| 加工级别 | 注塑级 | 特性级别 | 阻燃级,增强级 | 用途级别 | 汽车部件,电子电器部件,家电部件 |
特性:含有玻纤15%,强度大,难燃等级达1/32inch,UL94V-0,成型容易。
用途:连接器、冷却风扇、插座、线圈轴、汽机车零件、开关、电视机零件、整流器。
详细数据
订购指南
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
| 基本性能 | 吸水率 | --- | ASTM D-570 | 0.03 | % |
| 物理性能 | 成型收缩率 | --- | ASTM D-955 | 0.4-0.2 | % |
| 比重 | --- | ASTM D-792 | 1.50-1.52 | - | |
| 玻璃纤维含量 | --- | Ash | 15 | % | |
| 机械性能 | 引张强度 | --- | ASTM D-638 | 900-1100 | Kg/cm2 |
| 引张伸长率 | --- | ASTM D-638 | 4-5.5 | % | |
| 挠曲强度 | --- | ASTM D-790 | 1400-1800 | Kg/cm2 | |
| 挠曲弹性率 | --- | ASTM D-790 | 45000-65000 | Kg/cm2 | |
| IZOD冲击强度 | --- | ASTM D-256 | 5-7 | Kg.cm/cm | |
| 洛氏硬度 | --- | ASTM D-785 | 93 | M-Scale | |
| 电气性能 | 诱电率 | 60Hz | ASTM D-150 | 3.3 | --- |
| 诱电正接 | 60Hz | ASTM D-150 | 0.001 | --- | |
| 体积电阻率 | --- | ASTM D-257 | >1016 | Ω.cm | |
| 表面电阻率 | --- | ASTM D-257 | >1014 | Ω | |
| 绝缘破坏强度 | --- | ASTM D-149 | 22 | KV/mm | |
| 耐电弧性 | --- | ASTM D-495 | 90 | sec | |
| 热 性 能 | 耐燃性 | 0.75mm | UL 94 | V-0 | - |
| 热变形温度 | 4.6Kg/cm2 | ASTM D-648 | 220 | ℃ | |
| 线膨胀系数 | --- | ASTM D-696 | 5.5 | 10-5cm/cm℃ | |
| 熔点 | --- | DSC | 225 | ℃ | |
| 热变形温度 | 18.6Kg/cm2 | ASTM D-648 | 205 | ℃ | |